Acid Potassium Chloride Zinc Electroplating Softener
Solubilizing main brightener, auxiliary brightening effect, increase the coating thickness in low area, improve the depth capacity of the bath, reduce the surface tension of the bath, on the cathode surface wetting effect. The content in the bath is 25ml/L - 30ml/L The coating brittleness increases and passivation quality is affected by high content. The content is too low, the bright effect is not good, the coating is easy to flower, stay in the air and change color quickly.
Description
Acid potassium chloride zinc electroplating softener
Packing specifications: 25kg/plastic drum
200kg/plastic drum
1000kg/plastic drum on metal pallet
Payment: T/T or L/C
Delivery Port: Tianjin or Qingdao
Test Institution: SGS or CCIC
Capacity: 1000 MT per month
Period of Validity: 7 days
USE: 1. Metal surface treatment electro-galvanized
2. Galvanized standard parts, such as screw, nuts, and bolts
3. Metal accessories and metal fittings need to be galvanized
4. Electric galvanizing parts color has silver white, blue white, and color

Bath formula and technological parameters
|
|
concentration range |
Standard concentration |
|
KCl |
200-230 g/L |
220g/L |
|
ZnCl |
60-100 g/L |
60g/L (barrel) |
|
Boric Acid |
30-40 g/L |
35 g/L |
|
HL-93 Softening Agent |
20-30 g/L |
25 g/L |
|
HL-93 Brightening Agent |
0.6 ml/L- 1.0 ml/L |
0.8ml/L |
|
Temperature (℃) |
10-55℃ |
40℃ |
|
PH value |
4.8-5.6 |
5.2 |
|
DK (A/dm2) |
0.1-5 |
3 |

Hot Tags: acid potassium chloride zinc electroplating softener, China acid potassium chloride zinc electroplating softener manufacturers, suppliers, factory
Send Inquiry
You Might Also Like
-

Acid Potassium Chloride Zinc Electroplating Softener
-

Acid Potassium Chloride Zinc Electroplating Softener
-

Acid Potassium Chloride Zinc Electroplating Softener
-

Acid Potassium Chloride Zinc Electroplating Softener
-

Acid Potassium Chloride Zinc Electroplating Brightener
-

Acid Potassium Chloride Zinc Electroplating Softener